Analytical Instruments
Our laboratory is equipped with the latest analytical instrumentation from leading manufacturers worldwide.
ICP-MS
Inductively Coupled Plasma Mass Spectrometer for trace elemental analysis at ppb levels.
GC-MS
Gas Chromatography Mass Spectrometer for organic compound identification and quantification.
LC-MS
Liquid Chromatography Mass Spectrometer for complex mixture analysis and biomolecule characterization.
XRF Spectrometer
X-Ray Fluorescence for rapid, non-destructive elemental analysis of solids and liquids.
SEM / EDS
Scanning Electron Microscope with Energy Dispersive Spectroscopy for surface morphology and elemental mapping.
FTIR Spectrometer
Fourier Transform Infrared Spectrometer for molecular fingerprinting and functional group identification.
Mechanical Testing Equipment
Comprehensive mechanical testing capabilities for materials characterization.
Universal Testing Machine
100kN capacity UTM for tensile, compression, and flexural testing with environmental chambers.
Hardness Testers
Rockwell, Brinell, and Vickers hardness testing systems for metals and alloys.
Impact Tester
Charpy and Izod impact testing from -196°C to room temperature.
Thermal & Physical Analysis
DSC
Differential Scanning Calorimeter for thermal transitions and heat capacity measurements.
TGA
Thermogravimetric Analyzer for thermal stability and composition analysis.
DMA
Dynamic Mechanical Analyzer for viscoelastic properties and glass transition determination.